Reasons for making the exhaust system of the injection mold
The gas in the injection mold includes not only the air in the cavity, but also the air in the gate and the decomposition gas generated by the plastic melt, and the steam which caused by plastic in high temperatures. During injection molding, these gases should be exhaust in time, otherwise there will be some issues as following:
1. Defects such as flow mark, water mark, and weld marks will be formed on part surface;
2. Defects such as bubbles and loose tissues inside the plastic parts, which will lead to insufficient filling inside plastic part;
3. It is difficult to fill the plastic melt or flash locally;
4. The gas generates high temperature under high temperature and high pressure, causing local carbonization and burnt marks on the product;
5. Reducing the filling speed of the plastic melt, not only the molding cycle is prolonged, but the melt temperature decreases quickly after injection speed dropped, the residual stress will increase, if the injection pressure is increased, and the possibility of warping deformation of the plastic part after demolding will increase, if the material temperature is increased in order to reduce the injection pressure, it will cause the plastic to crack.

Properly making the exhaust slot can reduce the injection pressure greatly, reduce the injection and the holding time, and reduce the clamping pressure, thereby improving the production efficiency, reducing the production cost, and the energy consumption of the machine. For transparent plastic parts or plastic parts with strict surface requirements, we should be careful with the mold exhaust system design.

The air trapping position in cavity and exhaust method
Mar 2, 2022The air trapping in cavity is usually in the following places: 1. Thin-wall structure cavity, the end of melt flow; 2. The junction of two or more melts; 3. The last area where the melt in the cavity...view
Classification of side parting and core pulling mechanism
Jul 17, 2022According to the structural characteristics of plastic moulding, the side core-pulling mechanisms are divided into the following six categories: 1. The side core-pulling mechanism of "slider + guide...view
Venting insert design of molded parts
Mar 13, 2022In the thin-walled cavity, the end of the melt flow, the bottom of the blind hole of the mold cavity, the end of the solid column of the plastic part, the bottom of the plastic part rib and screw...view
Parting surface venting of runner system
Mar 10, 2022There are a large amount of gas in the main and sub channel, these gas are discharged through the pull rod (push rod) during injection processing, a part of gas come out from exhaust slot on parting...view
The sub gate of the plastic injection mold runner system
Jan 26, 2022In order to get the best injection quality, the gate type must be selected carefully, the coommon gate tyeps are: direct gate, side gate, pin-point gate, sub gate,valve gate of hot runner etc. Among...view
Gas-assisted injection molding product defects and solutions
Apr 28, 2022Common defects and solutions of gas-assisted injection moulding: 1. Gas blows out the melt like in picture 1. Reason: insufficient pre-filled amount. When the plastic part is a locally thickened...view